Item/Grade | Fire clay brick | ||||||
SK-30 | SK-32 | SK-34 | SK-35 | ||||
AL2O3% (≥) | 30 | 35 | 38 | 45 | |||
Fe2O3% (≤) | 2.5 | 2.5 | 2 | 2 | |||
Refractoriness(SK) | 30 | 32 | 34 | 35 | |||
Refractoriness under load, 0.2MPa, °C (≥) | 1250 | 1300 | 1360 | 1420 | |||
Apparent porosity (%) | 22-26 | 20-24 | 20-22 | 18-20 | |||
Bulk density (g/cm³) | 1.9-2.0 | 1.95-2.1 | 2.1-2.2 | 2.15-2.22 | |||
Cold crushing strength ,MPa (≥) | 20 | 25 | 30 | 40 |
Brands | DRN-125 | DRN-120 | RN-42 | RN-40 | RN-36 |
Al2O3 % | ≥45 | ≥42 | ≥42 | ≥40 | ≥36 |
Apparent Porosity % | ≤22 | ≤22 | ≤22 | ≤22 | ≤22 |
Bulk density g/cm3 | 2.15-2.35 | 2.00-2.00 | 2.00-2.20 | 2.00-2.20 | 2.00-2.20 |
Cold compressive strength MPa | ≥40 | ≥35 | ≥35 | ≥30 | ≥25 |
Refractoriness°C | ≥1760 | ≥1760 | ≥1760 | ≥1740 | ≥1700 |
Refractoriness under load°C | ≥1410 | ≥1350 | ≥1300 | ||
Creep rate%(0.2MPa*50h)≤ | 0.8 | 0.8 | |||
1250°C | 1200°C |